Typically UV, cold temps, or low quality plasticizer which....

Is likely the problem. The plasticizer can "off gas". The is increased by temps over 85 F and exposure fats, oils, and saliva. PVC is naturally brittle and the insulation on your ear phone leads are about 50% plasticizer.

Maybe put a sleeve on them....wash face before use....and wash leads after use???


Russ